http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-0173526-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4fa4c37b4aacb317ee027a1a729de4ff |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-235 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-521 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-181 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-29 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-181 |
filingDate | 1995-03-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 1999-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1999-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | KR-0173526-B1 |
titleOfInvention | Manufacturing method of elastic copolyester excellent in heat resistance and hydrolysis resistance |
abstract | This invention is a manufacturing method of the elastic copolyester excellent in heat resistance and hydrolysis resistance.n n n The present invention provides a carbodiimide compound, a phosphite compound, and an alkaline earth phosphorus to a copolyester of an aromatic dicarboxylic acid and a low molecular weight diol as a hard segment and an aliphatic polyester as a soft segment. A method of producing an elastic copolyester characterized by adding and kneading the compound. |