http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2020203367-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0068 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-139 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1395 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0585 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-043 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0562 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0562 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0585 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-139 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 |
filingDate | 2020-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2020203367-A1 |
titleOfInvention | All-solid-state secondary battery sheet and all-solid-state secondary battery manufacturing method, and all-solid-state secondary battery sheet and all-solid-state secondary battery |
abstract | A method for producing a sheet for an all-solid secondary battery containing a sulfide-based inorganic solid electrolyte having a volume average particle diameter of 1.0 μm or less and a particulate organic component, wherein the particle organic component and the volume average particle diameter are 1.0 μm or less. A mixture containing the sulfide-based inorganic solid electrolyte of the above and having a content of the particulate organic component of 15% by mass or less in the total content of the sulfide-based inorganic solid electrolyte and the particulate organic component. It includes pressurizing at a temperature higher than the glass transition temperature of the particulate organic component by 20 ° C. or more and lower than the decomposition temperature of the particulate organic component at a pressure higher than 1/10 of the elastic coefficient of the particulate organic component. , A method for manufacturing a sheet for an all-solid secondary battery, a method for manufacturing a sheet for an all-solid secondary battery, and a sheet for an all-solid secondary battery and an all-solid secondary battery. |