http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2020149385-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F293-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D153-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D153-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F293-00 |
filingDate | 2020-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2020149385-A1 |
titleOfInvention | Crosslinkable block copolymers and coating agents |
abstract | The present invention provides a crosslinkable block copolymer capable of forming a tough and tackless film, and a coating agent using the crosslinkable block copolymer. The crosslinkable block copolymer of the present invention contains a polymer block B and a polymer block A that contains a monomer unit that is bonded to each of both ends of the polymer block B and has crosslinkability, and is crosslinked. After that, when the attenuation curve obtained by the Solid echo method in 1 H pulse NMR (20 MHz) at 40 ° C. is fitted with a two-component relaxation curve using the nonlinear minimum square method, the shorter spin-spin relaxation time T. 2 (1) is 18 to 35 μsec, and the component ratio A 1 of the relaxation curve having the spin-spin relaxation time T 2 (1) is 40 to 70%. |
priorityDate | 2019-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |