http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2019216311-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2008-1095 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2207-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M8-0284 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L47-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0815 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M8-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 |
filingDate | 2019-05-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-04-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2019216311-A1 |
titleOfInvention | Rubber composition |
abstract | Ethylene / α-olefin copolymer having a melting point of 100 ° C. or higher and a glass transition temperature of Tg of -55 ° C. or lower was used in a proportion of 2.5 to 7.5 parts by weight per 100 parts by weight of ethylene / butene / diene copolymer rubber. Rubber composition. This rubber composition is a roll that retains the properties of ethylene-butene-diene copolymer rubber such as compression-resistant permanent strain resistance (95 ° C, 500 hours) and low-temperature elastic recovery test (evaluated by TR10 value and TR70 value). It is possible to improve workability such as workability and dough biting into a screw, and to maintain excellent compression-resistant permanent strain characteristics in an environment where a fuel cell is used. |
priorityDate | 2018-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |