abstract |
A polycarbonate resin (A) having a viscosity average molecular weight of 13,000 to 22,000, a terephthalic acid residue, a 1,4-cyclohexanedimethanol residue, and a 2,2,4,4-tetramethyl-1,3- A thermoplastic resin composition comprising: a thermoplastic resin component containing a polyester resin (B) containing a cyclobutanediol residue; and a glass filler (C). A total of 100 parts by mass of the polycarbonate resin (A) and the polyester resin (B) contains 25 to 65 parts by mass of the polycarbonate resin (A) and 75 to 35 parts by mass of the polyester resin (B), and 100 parts by mass of the thermoplastic resin component Contains 10 to 45 parts by mass of a glass filler (C). This thermoplastic resin composition is injection-molded with a heat-insulating mold or heat-cooled to produce a molded product. |