abstract |
The overall haze is 0.01 to 1.0%, the difference between the external hazes on both sides is 0 to 0.5%, the sine wave vibration is 1 Hz, and the heating rate is 3 ° C./min by the dynamic viscoelasticity measurement method. An acrylic resin film having a storage elastic modulus (E') at 23 ° C. measured under the above conditions of 1000 to 2200 MPa and a maximum loss tangent value (Tα) of 90 ° C. to 120 ° C. |