http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2019017380-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-13 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-68 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-42 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-70 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-68 |
filingDate | 2018-07-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-07-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2019017380-A1 |
titleOfInvention | Hybrid capacitor |
abstract | This hybrid capacitor is a hybrid capacitor in which the discharge capacity retention rate can maintain 80% or more for 1000 hours or more in a constant current constant voltage continuous charge test at 60 ° C. and 3.5 V, and is a positive electrode side and a negative electrode side The current collector is an aluminum material, the aluminum material is coated with an amorphous carbon film, the thickness of the amorphous carbon film is 60 nm or more and 300 nm or less, and the positive electrode contains graphite as a positive electrode active material, The negative electrode contains activated carbon as a negative electrode active material, and the activated carbon contains nitrogen. |
priorityDate | 2017-07-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |