http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2018168313-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02T10-86 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L71-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-02 |
filingDate | 2018-02-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2018168313-A1 |
titleOfInvention | Rubber composition for sidewall and pneumatic tire |
abstract | The present invention provides a rubber composition for a sidewall capable of improving low heat build-up, and a pneumatic tire using the same. The present invention provides a rubber component containing at least 30% by mass of an isoprene-based rubber, carbon black, a polyether having an average mass of two or more chains of ethylene oxide of at least 30% by mass of the total mass of ethylene oxide, and a polyether having at least 4 carbon atoms. A carbon black containing a zinc aliphatic carboxylate and / or a zinc aromatic carboxylate, wherein the carbon black has a content of 20 parts by mass or more based on 100 parts by mass of the rubber component and a CTAB specific surface area of 100 m 2 / g or less. The content of the black (1) is 50% by mass or more, and the content of the polyether is 20 parts by mass or less, based on 100 parts by mass of the rubber component, and the zinc aliphatic carboxylate and the zinc zinc aromatic carboxylate are contained. The rubber composition for a side wall having a total content of 20 parts by mass or less and a zinc oxide content of 10 parts by mass or less. |
priorityDate | 2017-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |