abstract |
A base material and an antifogging layer provided on at least a part of the base material, the antifogging layer containing a siloxane binder, silica particles, and a water-absorbing organic polymer, water absorption of the cloudy layer, 1.5 mg / cm 2 or more 25.0 mg / cm 2 or less, the water contact angle of the surface of the antifogging layer has 20 ° or less than 1 °, of the anti-fog layer The laminated body whose film thickness is more than 1 micrometer and is 10 micrometers or less, its manufacturing method, and the composition for anti-fogging coatings used suitably for formation of the said anti-fogging layer. |