abstract |
The present invention has a weight average molecular weight (Mw) of 200,000 or more and 3,000,000 or less, and has the most motion when approximating free induction decay at 130 ° C. measured by a solid-echo method of pulse NMR at three components. The ratio of the low-motility component (α130) is 40% or more and 60% or less, and the ratio β / γ of the intermediate motion component (β) to the highest mobility component (γ) is 1.0 or more and 4.0 or less. An ethylene polymer is provided. |