http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2018066670-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M50-105 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-02 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M50-105 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-34 |
filingDate | 2017-10-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2018066670-A1 |
titleOfInvention | Packaging material for battery, method for producing the same, and battery |
abstract | Provided is a battery packaging material having excellent formability. It is comprised from the laminated body provided with a base material layer, a barrier layer, and a heat fusible resin layer at least in this order, The base layer has at least a polyester film layer and a polyamide film layer, When the melting peak temperature of the polyester film layer is measured twice by differential scanning calorimetry, the melting peak temperature P (° C.) measured in the first heating and the melting peak measured in the second heating The packaging material for batteries whose difference with temperature Q (degreeC) is less than 5 degrees Celsius. |