http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2017199891-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B35-121 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1391 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-0471 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G53-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-131 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-364 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-131 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-1391 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-525 |
filingDate | 2017-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2017199891-A1 |
titleOfInvention | Non-aqueous electrolyte secondary battery positive electrode active material and method for producing the same, non-aqueous electrolyte secondary battery positive electrode mixture paste, and non-aqueous electrolyte secondary battery |
abstract | It aims at providing the positive electrode active material for nonaqueous electrolyte secondary batteries which can suppress gelatinization of the positive electrode mixture paste at the time of manufacturing a nonaqueous electrolyte secondary battery, and can improve stability. General formula LisNi1-x-yzCoxMnyMzO2 + α (where 0 ≦ x ≦ 0.35, 0 ≦ y ≦ 0.35, 0 ≦ z ≦ 0.10, 0.95 <s <1.30, 0 ≦ α ≦ 0.2, M is at least one element selected from V, Mg, Mo, Nb, Ti, W, and Al), and includes secondary particles formed by aggregation of primary particles. At least a part of the surface is coated with a lithium boron compound, and the amount of excess lithium hydroxide of the positive electrode active material measured by a neutralization titration method is 0.003% by mass or more and 0.5% by mass or less with respect to the entire positive electrode active material. Some positive electrode active materials. |