http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2017098892-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C49-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C49-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C43-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C43-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D81-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C49-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C43-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C49-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-06 |
filingDate | 2016-11-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2017098892-A1 |
titleOfInvention | Hollow container and method for producing the same |
abstract | An object of the present invention is to provide a hollow container excellent in barrier properties, suppressed in deformation of the container, and further excellent in strength, and a method for producing the same. In the hollow container of the present invention, 60 to 96 parts by mass of unmodified polyolefin (A), 1 to 20 parts by mass of acid-modified polyolefin (B), and 70 mol% or more of structural units derived from diamine are metaxylylenediamine. A polyamide (C) 3 containing a diamine unit derived from and a dicarboxylic acid unit derived from an α, ω-linear aliphatic dicarboxylic acid having 4 to 20 carbon atoms in which 70 mol% or more of the structural units derived from the dicarboxylic acid are derived. Using a resin composition containing 30 parts by mass (the total of unmodified polyolefin (A), acid-modified polyolefin (B) and polyamide (C) is 100 parts by mass), compression molding method, compression blow molding method Alternatively, it is formed by a compression stretch blow molding method, and has a portion where the polyamide (C) is dispersed in layers. |
priorityDate | 2015-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |