http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2016163282-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0587 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0566 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-587 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-505 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0587 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0566 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-052 |
filingDate | 2016-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-03-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2016163282-A1 |
titleOfInvention | Lithium ion secondary battery |
abstract | Provided is a lithium ion secondary battery that is excellent in safety and cycle characteristics and can suppress the rate of increase in resistance. A lithium ion secondary battery including a positive electrode, a negative electrode, and an electrolytic solution is manufactured. The positive electrode has a current collector and a positive electrode mixture applied to both sides of the current collector, and the positive electrode mixture is composed of a lithium / nickel / manganese / cobalt composite oxide and a lithium composite having an olivine structure. An oxide and a lithium-manganese composite oxide are included as a positive electrode active material. The negative electrode includes a current collector and a negative electrode mixture applied to both surfaces of the current collector, and the negative electrode mixture includes amorphous carbon as a negative electrode active material. |
priorityDate | 2015-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |