Predicate |
Object |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F136-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C19-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L91-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F36-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 |
filingDate |
2015-07-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2017-06-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-WO2016039004-A1 |
titleOfInvention |
Polybutadiene and rubber composition |
abstract |
In one embodiment of the present invention, the ratio (Tcp / ML 1 + 4 ) of 5% toluene solution viscosity (Tcp) measured at 25 ° C. to Mooney viscosity (ML 1 + 4 ) at 100 ° C. is 1.3 or more and 5.0 or less. Further, the present invention relates to a polybutadiene having a molecular weight distribution (Mw / Mn) of 2.0 or more and less than 4 and a cold flow rate (CF) of 5.5 mg / min or less. |
priorityDate |
2014-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |