http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2016017571-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-5357 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F1-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-4291 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-5357 |
filingDate | 2015-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-05-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2016017571-A1 |
titleOfInvention | Flame retardant resin composition and molded product therefrom |
abstract | A flame-retardant resin composition comprising 1 to 100 parts by weight of an organophosphorus compound (component B) represented by the following formula (1) with respect to 100 parts by weight of a polyolefin-based resin (component A). The resin composition has high flame retardancy, heat resistance and good physical properties. [Chemical 1] (In formula, X < 1 >, X < 2 > is the same or different, and is an aromatic substituted alkyl group represented by following formula (2).) [Chemical formula 2] (In the formula, AL is a branched or straight-chain aliphatic hydrocarbon group having 1 to 5 carbon atoms, and Ar is a phenyl group, naphthyl group or anthryl group which may have a substituent on the aromatic ring. N represents an integer of 1 to 3, and Ar can be bonded to any carbon atom in AL.) |
priorityDate | 2014-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |