http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2015156416-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2312-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2203-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-14 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0815 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 |
filingDate | 2015-04-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-04-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2015156416-A1 |
titleOfInvention | Resin composition, cross-linked product, and method for producing cross-linked product |
abstract | Provided are a resin composition that can easily give a crosslinked foam having excellent heat storage performance, a crosslinked product of the resin composition, and a method for producing the crosslinked product. Specifically, an olefin polymer having a main chain having a monomer unit based on ethylene and a branched chain having 5 or more carbon atoms, wherein the number of the branched chain constitutes the olefin polymer. The melting peak temperature observed by DSC is in the range of 20 to 40 ° C. within the range of 20 to 40 per 1000 carbon atoms, and the crystallization peak temperature observed by DSC Is in the range of 0 ° C. or higher and 40 ° C. or lower, and the melting enthalpy observed by DSC is 50 J / g or higher, and the melting peak temperature observed by DSC is in the range of 50 ° C. or higher and 180 ° C. or lower. A resin composition containing the olefin polymer as described above is provided. |
priorityDate | 2014-04-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |