http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2015137403-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L93-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J133-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09F1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J153-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 |
filingDate | 2015-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2015137403-A1 |
titleOfInvention | Adhesive composition and acrylic adhesive composition |
abstract | The present invention provides an adhesive composition that is substantially odorless, has excellent color tone, excellent adhesive properties or tack at a low temperature of about 5 ° C., and suppresses deterioration with time due to heat or light. Objective. The present invention is an adhesive composition containing a liquid rosin ester compound, and the liquid rosin ester compound is obtained by reacting a rosin compound with a monohydric alcohol compound having 1 to 10 carbon atoms. Yes, the Gardner color tone is 1 or less, the glass transition temperature is −20 ° C. or less, the esterification degree is 93% by weight or more, and the total peak area (Y) at the time of gas chromatography measurement under the following conditions It is related with the adhesive composition whose ratio (Y '/ Y) of peak area sum total (Y') of a retention time 16-22 minute area is 200 ppm or less. |