http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2015016257-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G45-1235 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-525 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G53-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G45-00 |
filingDate | 2014-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-03-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2015016257-A1 |
titleOfInvention | Method for producing lithium manganese-containing composite oxide |
abstract | Even when the sodium content of manganese dioxide is somewhat high, a lithium manganese-containing composite oxide with stable quality can be produced, and the distortion of the lithium manganese-containing composite oxide can be reduced. Propose manufacturing method. Manganese dioxide as a manganese raw material containing a sulfur (S) element and containing 0.1% by mass or more of a sodium (Na) element, a lithium raw material, and another metal raw material are mixed to form a raw material mixture composition And the molar ratio (S / Na) of S and Na contained in the raw material mixture composition is made higher than 0.4, and then the raw material mixture composition is fired at 500 ° C. or higher. A method for producing a lithium manganese-containing composite oxide is proposed. |
priorityDate | 2013-08-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |