http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2014092086-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2361-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2205-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2203-182 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2203-14 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G8-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-141 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0061 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-14 |
filingDate | 2013-12-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2017-01-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2014092086-A1 |
titleOfInvention | Phenolic resin foam and method for producing the same |
abstract | An object of the present invention is to obtain a phenolic resin foam having a low initial thermal conductivity and maintaining a low thermal conductivity over a long period of time. The present invention is a phenol resin foam containing a hydrocarbon having 6 or less carbon atoms and having a density of 10 kg / m 3 or more and 150 kg / m 3 or less, The hydrocarbon having 6 or less carbon atoms contains 60 to 10 mol% of cyclopentane in an amount of 40 to 90 mol% and one or more selected from hydrocarbons having a boiling point of -50C to 5C, The average boiling point X of hydrocarbons having 6 or less carbon atoms is 5 to 44 ° C., and the content Y of hydrocarbons having 6 or less carbon atoms in the phenolic resin foam is a spatial volume 22 in the phenolic resin foam. It is a phenol resin foam that is 0.25 to 0.9 mol per 4 × 10 −3 m 3 . |