http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2014041856-A1
Outgoing Links
Predicate | Object |
---|---|
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 |
filingDate | 2013-05-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2014041856-A1 |
titleOfInvention | Rubber composition, vulcanized product and molded product thereof |
abstract | Provided are a rubber composition from which a vulcanized product excellent in heat resistance can be obtained, and the vulcanized product and molded product thereof. Chloroprene rubber: 50 to 90% by mass and elastomer: 10 to 50% by mass of rubber component 100 parts by mass of zinc powder having an arithmetic average particle size of 3 to 10 μm measured by the method defined in JIS Z8901 A rubber composition is prepared by blending ˜20 parts by mass and 4 to 16 parts by mass of magnesium oxide having a BET specific surface area of 20 to 150 m 2 / g measured by a one-point method defined in JIS Z8830. Then, this rubber composition is molded and vulcanized to obtain a vulcanized product or a molded product. |
priorityDate | 2012-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 260.