http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2014002130-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3033 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B23-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 |
filingDate | 2012-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2016-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2014002130-A1 |
titleOfInvention | Polarizer |
abstract | An object of the present invention is to provide a polarizing plate that has high adhesion between layers and can suppress burrs when the polarizing plate is cut. The polarizing plate of the present invention has a thickness of 15 to 45 μm, and is disposed on a film containing cellulose ester, a cured resin layer disposed on one surface A of the film, and the other surface B of the film. A surface roughness Ra (A) of the one surface A of the film is 2.3 to 5.0 nm, and a surface roughness Ra (B) of the other surface B of the film is included. Is 1.0-3.0 nm, and the difference (Ra (A) -Ra (B)) between the surface roughness Ra (A) and the surface roughness Ra (B) is 0.3-2. 5 nm. |
priorityDate | 2012-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 196.