Predicate |
Object |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-0821 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-672 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08797 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08795 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-08755 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-092 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-0806 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-081 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-668 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate |
2013-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2016-02-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-WO2013187401-A1 |
titleOfInvention |
Polyester resin for toner, method for producing the same, and toner |
abstract |
The polyester resin for toner of the present invention contains 5 to 30% by mass of a structural unit derived from isosorbide and has a storage elastic modulus G ′ of 400 to 1000 Pa at 180 ° C. In the method for producing a polyester resin for toner according to the present invention, a mixture containing 5-30% by mass of isosorbide and polyvalent carboxylic acid is polycondensed at 230 ° C. or less, and polycondensation is performed at a softening temperature of 135-150 ° C. The reaction is terminated. |