http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2013146915-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-77 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3215 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3213 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3298 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2235-3236 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B35-475 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10N30-084 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10N30-097 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10N30-8536 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10N30-8561 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G29-006 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-187 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H03H3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-462 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-43 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-39 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-113 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H03H9-17 |
filingDate | 2013-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2015-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2013146915-A1 |
titleOfInvention | Piezoelectric ceramic, piezoelectric element, and method of manufacturing the piezoelectric ceramic |
abstract | PROBLEM TO BE SOLVED: To provide a piezoelectric ceramic having a small hysteresis of output charge output from the piezoelectric ceramic when a load is applied. [Solution] It has a pair of parallel main surfaces 2a and 2b located on the opposite side of the base 21 and side surfaces 4 connected to the peripheral edges 3a and 3b of the main surfaces 2a and 2b, respectively, and the composition formula is Bi 4 Ti 3 O. 12 · αMTiO 3 as a main component, M is at least one of Sr and Ba and 0.1 ≦ α ≦ 1 in the composition formula, and 0.1 ≦ α ≦ 1 is satisfied. X-ray diffraction using Cu—Kα rays with respect to the side surface 4 of the outer region 22, which includes an outer region 22 including the neighboring regions 4 A and 4 B of the surfaces 2 a and 2 b and an inner region 24 surrounded by the outer region 22. in the half-value width W a of peak diffraction angle (2 [Theta]) is in the range of 22.8 ° ~23.5 ° is, X-rays diffraction using Cu-K [alpha line for each main surface 2a and 2b of the inner region 24 In , To provide a piezoelectric ceramic 20, characterized in that the diffraction angles (2 [Theta]) is smaller than the half-value width W B of a peak in the range of 22.8 ° ~23.5 °. |