titleOfInvention | Anti-glare film and display device |
abstract | Provided is an antiglare film 1 having an improved antiglare property due to the generated sparkle. When the conditions regarding the surface unevenness of the antiglare film 1 having surface unevenness were A1 to A3 and the condition of the entire film was B, the antiglare film 1 was configured to satisfy (1) or (2). (1) Conditions A1, A2 and A3, (2) Conditions A1, A4 and B. Condition A1 has Rzjis (ten-point average roughness) of 3.4 μm or less. Condition A2 has an RΔq (root mean square slope) of 4? Condition A3 has an Ra (arithmetic mean roughness) of 0.3 μm or more. Condition A4 has an Rsm (average mountain interval) of 0.05 mm or more and 0.10 mm or less. Condition B has a haze value of 20% to 50%. The above numerical values under conditions A1 to A4 are all values measured according to JIS B0601: 2001. The above numerical values in Condition B are values measured in accordance with JIS K7136: 2000. |
priorityDate | 2011-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |