abstract |
The antifouling film is formed on the base and includes a binder component, conductive particles, and a fluororesin. The conductive particles are joined together by the binder component, and the binder component adheres to the base, and the surface of the conductive particles is made of the fluororesin. It has a covered membrane surface. |