http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2012127796-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G45-1257 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01D15-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G49-0027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G53-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G51-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-485 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G53-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G53-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G45-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-505 |
filingDate | 2012-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2014-07-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2012127796-A1 |
titleOfInvention | Method for producing lithium-containing composite oxide, positive electrode active material, and secondary battery |
abstract | Lithium that can synthesize lithium-containing composite oxides that contain one or more metal elements other than Li and Li, and whose crystal structure belongs to a layered rock salt structure, can suppress the formation of impurities under high-temperature and high-oxidation reaction conditions A method for producing a composite oxide containing: Theory of Li contained in a lithium-containing composite oxide containing 50 mol% or more of dehydrated lithium hydroxide composed of lithium hydroxide in a dehydrated state when the total amount of the metal-containing raw material containing the metal element is 100 mol% In a molten salt obtained by melting a molten salt raw material containing Li in a molar ratio exceeding the composition, a reaction at a reaction temperature of 350 ° C. or higher and a melting temperature of the molten salt raw material or higher; And a recovery step of recovering the lithium-containing composite oxide produced in the melt reaction step. |
priorityDate | 2011-03-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 100.