http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2012114396-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-016 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-04 |
filingDate | 2011-09-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2014-07-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2012114396-A1 |
titleOfInvention | Exterior body and method for manufacturing the same |
abstract | Resin component mainly composed of polylactic acid and / or lactic acid copolymer, and silica-magnesia catalyst particles as flame retardancy imparting component imparting flame retardancy, content of silica-magnesia catalyst particles flame retarded A flame retardant resin composition obtained by mixing so as to be 0.5 wt% or more and 9.0 wt% or less of the total weight of the curable resin composition is molded to form polylactic acid (PLA) and / or lactic acid co-polymer An exterior body of an electric device, which is a molded product of an environmental resin using a coalescence, is formed. The silica-magnesia catalyst particles preferably have an average particle size of 10 μm or less. |