http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2012070598-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-5313 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-5313 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-02 |
filingDate | 2011-11-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2014-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2012070598-A1 |
titleOfInvention | Polyamide resin composition |
abstract | A resin composition comprising a nylon 11 resin and / or a nylon 1010 resin (A1), a nylon 6 resin (A2), and a phosphorus flame retardant (B) containing no halogen element, the nylon 11 resin And / or the mass ratio (A1: A2) of the nylon 1010 resin (A1) and the nylon 6 resin (A2) is 1: 4 to 4: 1 and the content of the phosphorus-based flame retardant (B) containing no halogen element Is 15 to 60 parts by mass with respect to 100 parts by mass of the total amount of nylon 11 resin and / or nylon 1010 resin (A1) and nylon 6 resin (A2), and the melt viscosity of nylon 6 resin (A2) is 5 A polyamide resin composition having a viscosity of ˜170 Pa · s. |