http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2012046848-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B1-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B1-244 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K23-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J2-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J2-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B1-243 |
filingDate | 2011-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2014-02-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2012046848-A1 |
titleOfInvention | Method for producing granulated product of iron ore raw material and granulated product of iron ore raw material |
abstract | The method for producing a granulated product of this iron ore raw material has a polymer surface activity having a hydrophobic group and an acidic functional group and a molecular weight of 10,000 to 30,000 with respect to 100 parts by mass of the total amount of iron ore raw material consisting of fine iron ore. A step of adding 0.01 to 10 parts by mass of an agent, one or two of CaO and Ca (OH) 2 in terms of Ca (OH) 2 and a total of 0.5 parts by mass and 3 to 25 parts by mass of water including. |