Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2495 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31909 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-3192 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D10B2401-046 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2224-32225 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2224-73204 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L2224-16225 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D02G3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D31-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L23-373 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-426 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D02G3-045 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-30 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-32 |
filingDate |
2011-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2013-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-WO2012026119-A1 |
titleOfInvention |
Shape-retaining film and manufacturing method thereof, laminated film / tape, adhesive film / tape, anisotropic heat conductive film, and shape-retaining fiber |
abstract |
An object of the present invention is to provide a shape-holding film that is excellent in shape-retaining properties, has a high tensile elastic modulus, and has good longitudinal tear resistance. At least one base material layer including an ethylene polymer having a density of 900 kg / m 3 or more and a weight average molecular weight (Mw) / number average molecular weight (Mn) of 5 to 20, and at least one layer including a polymer material The ethylene-based polymer is an ethylene homopolymer or an ethylene-α-olefin copolymer having a C 3-6 α-olefin unit content of less than 2% by weight, The polymer material has a melting point Tm2 lower than the melting point Tm1 of the ethylene polymer, a tensile elastic modulus of 10 to 50 GPa, and a return angle by a 180 ° bending test of 65 ° or less. |
priorityDate |
2010-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |