http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2011108514-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G83-007 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-333 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G81-00 |
filingDate | 2011-03-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2013-06-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2011108514-A1 |
titleOfInvention | Material having crosslinked polyrotaxane and method for producing the same |
abstract | The present invention provides a material having high flexibility and high dielectric constant and a method for manufacturing the same. The present invention is a material having a first polyrotaxane and a second polyrotaxane, wherein the opening of the first cyclic molecule is clad in a skewered manner by the first linear molecule. The first blocking group is arranged at both ends of the first pseudopolyrotaxane to prevent the first cyclic molecule from leaving, and the second polyrotaxane has an opening of the second cyclic molecule in the second straight chain. A second blocking group is arranged at both ends of the second pseudopolyrotaxane clathrated by the chain molecules so that the second cyclic molecule is not detached, and the first and second polyrotaxanes Provides a material as described above, wherein the material is crosslinked via first and second cyclic molecules, the material is solvent free, and the material has a dielectric constant of 1 kHz or greater at 6.0 kHz. |
priorityDate | 2010-03-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links