http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2010061917-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2333-06 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L35-00 |
filingDate | 2009-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2012-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2010061917-A1 |
titleOfInvention | Optical film and manufacturing method thereof |
abstract | Provided are an optical film mainly composed of an acrylic resin having a ring structure in the main chain, which has both sufficient transparency as an optical film and anti-blocking property, and a method for producing the same. An optical film containing an amorphous acrylic resin (A) having a ring structure in the main chain as a main component and particles (B), formed by melt extrusion, and satisfying the following conditions (i) to (iii) (I) The total light transmittance measured in accordance with JIS K7361 is 90% or more and the haze is 1% or less; (ii) The ten-point average roughness Rz of the surface measured in accordance with JIS B0601 is 1.0 μm or more; (iii) The number of bending resistances (MIT times) measured in accordance with JIS P8115 is 100 times or more. |