titleOfInvention | Acid galvanizing bath |
abstract | Provided is an acidic galvanizing bath having improved stability over time even at a high temperature of 30 to 50 ° C. An acidic zinc plating bath containing a conductive salt, metallic zinc, and a brightening agent, and containing at least one cumylphenol anionic surfactant as a component of the brightening agent. |