http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2010007970-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-7792 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-7734 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-64 |
filingDate | 2009-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2012-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2010007970-A1 |
titleOfInvention | Method for producing long afterglow phosphor |
abstract | Provided is a method for producing a MAl 2 O 4 : Eu type long afterglow phosphor capable of reducing raw material costs. Manufacturing of MAl 2 O 4 : Eu type long afterglow phosphor (M is alkaline earth metal) characterized by mixing and baking a BAM (alkaline earth aluminate) phosphor and an alkaline earth compound Method. |
priorityDate | 2008-07-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |