http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2009148138-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-0274 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C33-424 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C33-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C59-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-0002 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C59-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C33-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C33-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C33-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L21-027 |
filingDate | 2009-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2011-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2009148138-A1 |
titleOfInvention | NANOIMPRINT MOLD, PROCESS FOR PRODUCING THE SAME, RESIN MOLDED ARTICLE HAVING FINE Roughness Structure on Surface, AND METHOD FOR PRODUCING WIRE GRID POLARIZER |
abstract | A nanoimprint mold that can accurately transfer a fine concavo-convex structure, is inexpensive, and has high durability, a manufacturing method thereof, a resin molded body having a fine concavo-convex structure on a surface onto which the fine concavo-convex structure of the mold is accurately transferred, and a wire grid Provided is a method by which a type polarizer can be produced with high productivity. A mold for nanoimprint having a fine concavo-convex structure composed of a plurality of grooves 14 formed in parallel to each other at a constant pitch on the mold surface, and made of a resin having a fine concavo-convex structure on the surface as a base of the fine concavo-convex structure A nanoimprint mold 10 having a mold base 12, a metal oxide layer 16 covering the surface of the mold base 12 having a fine relief structure, and a release layer 18 covering the surface of the metal oxide layer 16 is used. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9806229-B2 |
priorityDate | 2008-06-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 156.