http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2009116308-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-27 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C2005-145 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0846 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-283 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B25-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B60C1-0008 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B25-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-28 |
filingDate | 2009-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2011-07-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2009116308-A1 |
titleOfInvention | Laminated body and pneumatic tire using the same |
abstract | Provided are a laminate excellent in adhesiveness between a thermoplastic resin composition layer and a rubber adhesive layer, and further in durability during use, and a pneumatic tire including the laminate. This laminate is a laminate comprising a thermoplastic resin composition layer and a rubber composition layer, and the thermoplastic resin composition layer comprises an ethylene-vinyl alcohol copolymer having an ethylene unit content of 20 to 50 mol%. The rubber composition layer comprises at least one selected from the group consisting of a polymer, an aliphatic polyamide having a molar ratio of methylene groups to amide groups of less than 5.4, and a metaxylenediamine-adipic acid polycondensate, 30 to 120 parts by weight of wet silica having a BET specific surface area of 100 to 300 m 2 / g is included with respect to 100 parts by weight of the rubber component. |