titleOfInvention | Method for producing vinyl resin |
abstract | In the present invention, in the suspension polymerization of a vinyl compound using a polymerization tank equipped with a reflux condenser, the obtained vinyl polymer particles are uniform, and defoaming properties against dry foam generated in the middle to late stages of polymerization are obtained. Provided is a method for producing an excellent vinyl resin. The present invention uses a polymerization tank equipped with a reflux condenser to perform suspension polymerization of a vinyl compound in the presence of a dispersion stabilizer for suspension polymerization. With respect to 100 parts by weight of the compound, the side chain has an unsaturated double bond, an aromatic group optionally having a carboxyl group, a saturated aliphatic group having a carboxyl group, or a saturated aliphatic group having 11 or more carbon atoms A vinyl alcohol polymer (A) having a content of 0.001 to 5 parts by weight is added. |