http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2008108428-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G21K2004-12 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G21K4-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G21K4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01T1-20 |
filingDate | 2008-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2010-06-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2008108428-A1 |
titleOfInvention | Scintillator panel and method for manufacturing scintillator panel |
abstract | In the present invention, even when a large-sized flexible resin substrate is used, the deformation of the substrate does not increase, it is easy to handle, the phosphor layer is damaged due to the large deformation of the substrate, the image quality is improved. A scintillator panel using a flexible resin substrate that does not have a problem of deterioration and a method of manufacturing the scintillator panel are provided. The scintillator panel of the present invention has a phosphor layer having a thickness of 100 μm or a weight of 45 mg or more per 1 cm 2 on a flexible resin substrate, and the long side of the flexible resin substrate is acm, When the short side is bcm, the thickness of the flexible resin substrate is set to 75 × {a 2 / (10 × b)} 1/3 μm to 1000 μm. |