http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2008001709-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-7815 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-0045 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2229-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G2300-1059 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G2300-202 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2229-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2229-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G2400-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G2300-301 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J29-166 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G11-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C10G11-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-0006 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J29-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10G11-05 |
filingDate | 2007-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2009-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2008001709-A1 |
titleOfInvention | Desulfurization function-added fluid catalytic cracking catalyst, method for producing the same, and method for producing low sulfur catalytic cracking gasoline using the desulfurization function-added fluid catalytic cracking catalyst |
abstract | In the process of producing catalytic cracking gasoline by cracking heavy oil, (a) alumina-coated zeolite and (b) porous inorganic other than zeolite, which can efficiently reduce the sulfur content in the catalytic cracking gasoline It is a catalyst formed by supporting vanadium on a support made of an oxide and / or clay mineral, or (a) containing 5 to 40% by mass of zeolite coated with alumina and (b) 30 to 70% by mass of alumina. The support is supported by vanadium, and the ratio of vanadium concentration before and after pulverization is a catalyst of 2 or more, or the support containing a porous inorganic oxide supports at least vanadium and manganese and / or phosphorus. And vanadium and manganese and / or phosphorus form a composite ion in the supporting solution when supporting vanadium and manganese and / or phosphorus, Transmission of the reverse osmosis membrane merging ions, to provide a catalyst is not more than 25 wt% with respect to the transmission of the reverse osmosis membrane of vanadium. |
priorityDate | 2006-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |