http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2007114062-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-06 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16F15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16F1-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 |
filingDate | 2007-03-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2009-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2007114062-A1 |
titleOfInvention | Rubber composition and rubber cross-linked product |
abstract | The main object of the present invention is to provide a rubber composition that can be a rubber cross-linked product having high vibration damping properties and excellent compression set resistance. In order to achieve the above object, the present invention provides 100 parts by mass of a rubber component (A) having crosslinkability, and 10 to 100 parts by mass of a thermoplastic elastomer (B) comprising an aromatic vinyl-conjugated diene block copolymer. And 0.1 to 10 parts by mass of a crosslinking agent (C) capable of crosslinking only the rubber component (A), and the storage elastic modulus G ′ at 0 ° C. is 1 × 10 6 Pa or less. A rubber composition is provided. |
priorityDate | 2006-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 136.