http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2007081014-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61F7-032 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K5-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61F7-08 |
filingDate | 2007-01-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2009-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2007081014-A1 |
titleOfInvention | Method and apparatus for producing hydrous exothermic composition |
abstract | By continuously dispersing and feeding the components into small compartments and continuously mixing and conveying the components, a heat generating composition containing a heat generating water amount or a water amount higher than that at a stable composition ratio can be obtained at a necessary time. A custom-made exothermic composition manufacturing method and manufacturing apparatus are provided. A method for producing a hydrous exothermic composition for producing a raw material of an exothermic composition containing iron powder, a carbon component, a reaction accelerator and moisture as essential components, wherein the cylindrical shape is disposed in a laterally arranged cylindrical body. A step of measuring and supplying the powder raw material into the body, a step of conveying the powder raw material while mixing, a step of measuring and supplying the liquid raw material, and a step of conveying while mixing the powder and the liquid Are performed in order. |