http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2007072595-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0587 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-131 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G51-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G53-00 |
filingDate | 2006-06-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2009-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2007072595-A1 |
titleOfInvention | Nonaqueous electrolyte secondary battery |
abstract | A positive electrode including a positive electrode mixture and a positive electrode current collector carrying the same, a negative electrode, a separator including a polyolefin resin, a non-aqueous electrolyte, and a non-aqueous electrolyte secondary battery including a heat-resistant insulating layer. The estimated heat generation rate at 200 ° C. is 50 W / kg or less. The positive electrode and the negative electrode are wound together with a separator and a heat-resistant insulating layer interposed therebetween. |
priorityDate | 2005-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |