http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2007029497-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-04 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 |
filingDate | 2006-08-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2009-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2007029497-A1 |
titleOfInvention | Thermoplastic resin composition, conductive film and conductive sheet |
abstract | By blending the modified conjugated diene polymer with a styrene resin and conductive carbon, the conductive carbon does not fall off, and a thermoplastic resin composition having an excellent balance of impact resistance, low-temperature characteristics, and conductivity, and comprising the same A conductive film and a conductive sheet are provided. (Ii) 2.5 to 35 parts by weight of a modified conjugated diene polymer having at least one group selected from the group consisting of an alkoxysilyl group, an amino group, an acid anhydride group, and a carboxyl group, and (b) impact resistance. (C) 40 to 90 parts by weight of non-rubber-modified styrene polymer, and (d) 1 to 15 parts by weight of conductive carbon [However, (A) + (B) + (C) + (d) = 100 parts by weight], and a conductive film and a conductive sheet formed by molding the thermoplastic resin composition. |