http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2007013232-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D2701-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-14 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C26-00 |
filingDate | 2006-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2009-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2007013232-A1 |
titleOfInvention | Pre-coated metal plate and manufacturing method thereof |
abstract | The present invention provides a precoated metal sheet that is excellent in corrosion resistance and has excellent design in appearance because a vivid color can be expressed even if the coating thickness is reduced in order to prevent occurrence of boiling defects, and a method for producing the same. The pre-coated metal plate is a multi-layer pre-coated metal plate in which a multi-layer coating film is formed by sequentially laminating a primer coating layer, an intermediate coating layer film and a top coating layer on one side or both sides of a metal plate, The primer coating layer contains one or both of Si and P, and there is a liquid interface trace interface between the intermediate coating layer and the top coating layer in the multilayer coating, and the liquid interface trace The size of the fine irregularities at the interface is 0.3 to 0.8 μm expressed by the center line average roughness (Ra), and the intermediate coating layer contains a Ti-based additive. |
priorityDate | 2005-07-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |