http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2006106680-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02T10-70 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-042 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-38 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-42 |
filingDate | 2006-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2008-09-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2006106680-A1 |
titleOfInvention | Electrode material for electric double layer capacitor, manufacturing method, electrode for electric double layer capacitor, and electric double layer capacitor |
abstract | Good moldability, high bending resistance after molding to the active material layer and high adhesion to the current collector, increasing the capacitance of the electric double layer capacitor using the active material layer obtained by molding, Provided are an electrode material for an electric double layer capacitor capable of reducing internal resistance, and an electrode for an electric double layer capacitor and a capacitor obtained by using the electrode material. An electrode material for an electric double layer capacitor is composed of a mixture particle containing a binder and an electrode active material. In the mixture particle, 50% by area or more of the surface of the mixture particle is coated with the binder. . |