http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2006104092-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2924 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-298 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-914 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L101-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-912 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3477 |
filingDate | 2006-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2008-09-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2006104092-A1 |
titleOfInvention | RESIN COMPOSITION, MOLDED BODY, AND METHOD FOR PRODUCING THEM |
abstract | By adding at least one compound represented by the general formula (I) to a resin composition containing an aliphatic polyester resin having a carboxyl group at the molecular chain terminal, a part of the carboxyl group at the molecular chain terminal is added by the compound. Alternatively, the amount of the compound represented by the general formula (I) is 0 by mixing a resin composition containing an aliphatic polyester resin that is entirely blocked and a pellet made of an aliphatic polyester resin having a carboxyl group at the end of the molecular chain. 1. A fiber production method characterized by adjusting to 1 to 8% by weight, spinning temperature 200 to 250 ° C., melt residence time 180 to 1800 sec, spinning speed 500 to 10000 m / min. [Chemical 1] (Here, at least one of R 1 to R 3 is a glycidyl group, and the rest represents hydrogen, an alkyl group having 1 to 10 carbon atoms, a hydroxyl group, and an allyl group.) |