http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2006088203-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133502 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-26 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133502 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-111 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-02 |
filingDate | 2006-02-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2008-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2006088203-A1 |
titleOfInvention | Optical laminate manufacturing method and manufacturing apparatus |
abstract | The present invention discloses an antiglare laminate capable of realizing excellent glare prevention and black reproducibility (representing black gradation at low luminance) while having antiglare properties. The present invention is a method for producing an optical laminate comprising a light transmissive substrate and an antiglare layer formed on the light transmissive substrate, the light transmissive substrate being prepared, Forming the antiglare layer having a concavo-convex shape on the light-transmitting substrate, and the concavo-convex shape of the antiglare layer is defined as Sm as an average interval of the concavo-convexity of the antiglare layer, Sm is 100 μm or more and 600 μm or less, θa is 0.1 degree or more and 1.2 degree or less, and Rz is 0. 0, where the average inclination angle of the uneven part is θa and the average roughness of the uneven part is Rz. It is defined as exceeding 2 μm and not exceeding 1 μm. |