http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2006054410-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-48 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-48 |
filingDate | 2005-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2008-05-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2006054410-A1 |
titleOfInvention | Method for producing imide resin, and imide resin and imide resin molded article obtained thereby |
abstract | An object of the present invention is a method for producing an imidized acrylic resin that is excellent in transparency and heat resistance, is less likely to cause optical distortion (birefringence) even under molding stress, and has few imidation-derived foreign substances, and It is to provide an imidized acrylic resin molded body made of them. The method for producing an imidized acrylic resin of the present invention is a production method in which a (meth) acrylic ester resin is treated with an imidizing agent in the presence of a heat stabilizer, and is 210 mm long, 300 mm wide, and thick. This is a method for producing an imide resin in which the total number of imidization-derived foreign substances contained in a 3 mm molded body is 100 or less. |