http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2006025293-A1
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2365-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2345-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-14 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L65-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 |
filingDate | 2005-08-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2008-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-WO2006025293-A1 |
titleOfInvention | Method for producing resin composition |
abstract | A process for producing a resin composition comprising melt-kneading a cyclic olefin polymer (A) having a glass transition temperature of 60 to 200 ° C and a soft polymer (B) having a glass transition temperature of 0 ° C or lower, wherein the cyclic olefin polymer Production of a resin composition in which a part of (A), a soft polymer (B), and a radical initiator (C) are previously melt-kneaded and then the remaining cyclic olefin polymer (A) is added and melt-kneaded. Provide a method. By blending the cyclic olefin polymer (A) twice, the mixture having a crosslinked structure can be diluted with the cyclic olefin polymer (A) having no crosslinked structure, and the melt viscosity is increased. Can be suppressed. And the resin composition excellent in abrasion resistance and melt moldability is obtained. |